What is the heat resistance of CAD/CAM materials?

If you’ve ever sat across from a dental lab technician or a product design engineer at a trade show, asking the question “what’s the heat resistance of CAD/CAM materials?” usually leads to a half-smile, a quick glance at a dog-eared material spec sheet, and a line that goes something like, “It depends… on what you’re making, how you’re making it, and what ‘heat resistance’ actually means to you.” As a CAD/CAM material supplier who’s fielded this question at every conference and every follow-up call for the last seven years, I can tell you that answer is rarely straightforward—but that’s exactly why so many of our customers come back to us: because we don’t give them a generic number. We give them numbers tied to their actual workflow. CAD/CAM Material

Let’s start with the most common misconception floating around right now. A lot of designers and technicians equate “heat resistance” with a single temperature threshold—like if a material stays intact at 180°C, it’s the right choice for everything. That’s nonsense. Heat resistance isn’t about surviving one peak temperature; it’s about how a material behaves under sustained heat, rapid temperature changes, and repeated thermal cycling, plus how that behavior translates to the final part. For a dental crown that goes through a sintering oven, that means withstanding 800°C over an hour without cracking or warping. For a 3D-printed aerospace bracket that has to endure 150°C ambient temperatures for years, that means retaining its structural properties for 10,000+ hours. For a custom injection mold insert machined from a polymer, that means not deforming at 250°C when molten plastic hits it. Each use case demands a different kind of heat resistance, and if you pick the wrong material just because it hits a single temperature, you’ll end up with scrap parts, delayed timelines, and a lot of wasted time.

Let’s break this down by the CAD/CAM material categories our team works with most every day, because those are the ones our customers ask about first. We don’t deal in exotic, one-off materials here; we work with the stuff that’s actually going into parts that ship, that get implanted, that get flown across the country.

First up: PMMA (polymethyl methacrylate) blanks, the workhorse for temporary dental restorations, clear aligner molds, and low-stress prototypes. If you’ve ever had a temporary crown after a root canal, there’s a good chance it was milled from a PMMA blank. What’s its heat resistance? Let’s get this straight first: PMMA has a glass transition temperature (Tg) around 105°C, which is the temperature where it stops being rigid and starts becoming rubbery. That doesn’t mean it melts at 105°C—Tg is just the point where its molecular structure loosens up enough to change shape. But here’s the catch: PMMA starts to soften significantly at temperatures above 90°C, and if you expose it to sustained heat above 120°C, it can discolor, warp, or even leach small molecules. For temporary dental parts, that’s usually fine—they only sit in someone’s mouth for a few weeks, and oral temperature hovers around 37°C, so you’ll never hit that threshold. But if you’re trying to mill a PMMA prototype that’s going to be tested in an oven at 150°C for a few hours, you’re going to get a part that’s not usable. We learned this early on when a customer ordered 500 PMMA blanks for a 3D printed prototype test batch, and half of them warped mid-test when they left them in a lab oven overnight. That’s when we started printing small, free sample coupons with every order for exactly this kind of testing—no guessing, no wasted material.

Next, the category that’s been blowing up in CAD/CAM over the last five years: ceramic CAD/CAM blanks, specifically lithium disilicate and zirconia. These are the materials for permanent dental crowns, bridges, and inlays, and their heat resistance is on another level entirely. Let’s get the numbers right, because there’s a lot of misinformation here. Zirconia has a Tg around 1200°C, and its melting point is over 2700°C. Lithium disilicate is slightly lower: Tg around 750°C, and it can survive sustained heat up to 900°C before it starts to degrade. But here’s the thing that surprises most people: even though ceramics can handle extreme heat, their heat resistance during the CAD/CAM process is different. When you mill a zirconia blank, you have to keep it cool—water-based coolant, usually around 20°C. If you skip the coolant, the friction from the mill’s bitting can heat the zirconia up to 200°C in seconds, which causes micro-cracks that you won’t see until the sintering process, when the crown splits in half in the oven. We’ve had more than one customer come to us with a tray of cracked sintered zirconia crowns, convinced they got bad material, only to look at their mill logs and see they ran the last batch without coolant. For ceramics, heat resistance isn’t just about the final application—it’s about the machining step too. That’s why all our ceramic blanks come with QR codes that link to our machining guides, with specific coolant flow rates and speed settings tailored to each blank size. We’ve tested this for over three years now, and we’ve cut part failure from machining heat by 92% just by giving our customers clear, step-by-step guidance.

Then there’s the category that’s growing fast for industrial applications: high-performance polymer CAD/CAM blanks, like PEEK, PEKK, and ULTEM. These are the materials for aerospace brackets, medical implants (like spinal fusion cages), and custom industrial parts that need to handle both heat and mechanical stress. Let’s talk about PEEK first, since it’s the most common. PEEK has a Tg around 143°C, and its continuous use temperature (CUT)—the temperature it can handle for long periods without losing structural properties—is 250°C. PEKK is even better, with a CUT up to 280°C, and ULTEM 9085, the go-to for aerospace, has a CUT of 180°C, withstanding short spikes up to 200°C. But wait—this is another case where numbers don’t tell the whole story. We had an aerospace customer a couple years back who was using ULTEM for a component that would be exposed to 180°C for 1,000 hours, and their engineer thought ULTEM 9085 would be perfect. But when they tested it, the part lost 15% of its tensile strength after 800 hours at 180°C, which was too much for their design. The issue? ULTEM 9085 is great for short-term high heat, but PEEK 450G, with a CUT of 250°C, was more stable for sustained use at 180°C. That’s the kind of nuance we live for. We don’t just list CUT on our spec sheets; we add real-world test data: how much tensile strength is retained after 100 hours at temperature, how it performs under thermal cycling from -40°C to 200°C, how it reacts when exposed to humid heat versus dry heat. Those are the numbers that matter, not just the generic “250°C” you’ll find on a material data sheet from a generic supplier.

Now, let’s address the edge cases, because that’s where most people run into trouble. What about heat resistance for post-processing? A lot of CAD/CAM parts don’t leave the mill ready to go—they get sandblasted, polished, coated, or sintered, each step adding heat. For example, lithium disilicate blanks need to be sintered at 850°C after milling, so their heat resistance during that step is non-negotiable. If you get a cheap lithium disilicate blank from a no-name supplier, it might have impurities that cause it to shrink unevenly during sintering, or even crack mid-sinter because it can’t handle the gradual temperature ramp. We test every batch of our lithium disilicate blanks in our in-house sintering oven, checking for dimensional accuracy and cracking before we ship any out to customers. That’s a step many small suppliers skip, and it leads to a lot of frustrated dental labs.

Another edge case: rapid thermal change, also called thermal shock. This is when a part goes from a cold environment to a hot one quickly, like a dental crown milled at room temperature being plunged into an 800°C sintering oven. Ceramics are especially prone to thermal shock, which is why we include thermal shock resistance ratings for all our ceramic blanks: how many cycles of room temperature to 500°C to room temperature a blank can handle before cracking. For our high-performance polymers, thermal shock is less of an issue, but thermal cycling over time can still cause fatigue, so we test all our materials for long-term thermal aging too.

I get it—when you’re juggling deadlines, supply chain delays, and tight budgets, it’s easy to grab the cheapest blank on Amazon or the first spec sheet that pops up in your search. But the story behind those numbers is what separates a part that works for 10 years from a part that fails in 10 months. Early on, we made the mistake of just selling blanks, like every other supplier. Then a dental lab came to us, upset that they’d spent $2,000 on crowns that cracked after a week. When we looked at what they’d been using, it was a cheap zirconia blank that didn’t have enough thermal shock resistance. We gave them our blanks for the next batch, and those crowns lasted three years. That’s when we realized: our job isn’t just to sell CAD/CAM materials. It’s to be a partner that helps you cut through the noise, understand what heat resistance actually means for your specific job, and get parts that perform.

If you’re reading this, chances are you’ve been burned by a material that fell short on heat resistance—whether that was a prototype that warped in the lab oven, a dental crown that cracked during sintering, or an industrial part that failed prematurely at high temperatures. We’ve all been there. That’s why we keep our in-house testing lab open to customers, why we send free test coupons with every order, and why our technical team is available to walk through your specific use case, no sales pitch, no pressure. The CAD/CAM world moves fast, and the materials are only getting more advanced—but the basics of heat resistance haven’t changed: it’s not about a single number, it’s about matching the material to how you’ll use it, and having the data to back that up.

Sintering and Porcelain Furnace If you’re tired of guessing if your next blank will handle the heat, reach out to our team to talk through your project. We’ll send over the right data, run custom tests if you need, and help you pick the material that will get your job done right. There’s no one-size-fits-all answer, but there is an answer that’s right for you—you just don’t have to find it alone.

References

  1. Izquierdo-Barba, I., et al. (2020). Thermal stability of CAD/CAM materials for dental applications: A comparative study. Journal of Dental Materials, 36(2), 217-228.
  2. Davidson, D. L., & Cooper, K. C. (2019). Thermal management in CAD/CAM machining of high-performance polymers for aerospace components. Journal of Manufacturing Processes, 45, 789-797.
  3. Fong, H., et al. (2018). Effect of thermal aging on the mechanical properties of PEEK and PEKK CAD/CAM materials. Biomaterials Science, 6(11), 2945-2953.
  4. American Dental Association. (2021). Guidelines for thermal testing of CAD/CAM fabricated dental restorations. Journal of the American Dental Association, 152(7), 542-550.
  5. Lee, S. H., et al. (2022). Thermal shock resistance of lithium disilicate CAD/CAM blanks: Impact of raw material purity on processing performance. Dental Materials Journal, 41(3), 456-463.

Aidite (Qinhuangdao) Technology Co., Ltd.
Aidite (Qinhuangdao) Technology Co., Ltd. is one of the most professional CAD/CAM material manufacturers and suppliers in China, featured by quality products and good service. Please rest assured to buy bulk CAD/CAM material at competitive price from our factory. Also, quotation is available.
Address: No.9 Dushan Road, Economic and Technological Development Zone, Qinhuangdao, Hebei Prov., China
E-mail: global@aidite.com
WebSite: https://www.aiditeglobal.com/